1.2316

Description

Chemical Composition

CCrMo
0,3816,501,20

Steel properties

Stainless martensitic steel with increased Cr-content for improved corrosion resistance. This grade is usually
supplied in a quenched and tempered condition. Good polishability.

Applications

Tools and moulds for corrosive plastics and polymers, food industry.

Condition of delivery

Quenched and tempered, 750 – 950 N/mm²

Physical properties

20-100°C   20-200°C   20-300°C   20-400°C
 10,3	     10,8	11,2	   11,6
 
Thermal conductivity
[w/m.k]  20°C /19.6  350°C / 21,1
 
TemperatureCoolingHardness
760 - 800°Cfurnacemax. 230 HB
TemperatureCoolingTempering
1020 - 1050°Coil, pressure gas (N2), air or hot bath 500 - 550°Csee tempering diagram
TemperatureCooling
500 - 550°Cfurnace

(1.2316) Thermal Cycle Diagram